Home
/
Categories
/
Chemicals
/
Paint & Coatings
/
Other Paint & Coatings
/
101 Metal-Filled Epoxy Putty Repair Adhesive, Casting Defect Rebuilding Putty
101 Metal-Filled Epoxy Putty Repair Adhesive, Casting Defect Rebuilding Putty
FOB Price 7.5 - 8 USD / Set
MOQ
1000 Set
Port
Shanghai
Lead Time
7 days
China
Main Products : gasket maker, acrylic ab glue, epoxy steel, potting compound
Tanxi Road No.6, Xiangcheng District Xiangfan, Hubei
101 Metal-Filled Epoxy Putty Repair Adhesive, Casting Defect Rebuilding Putty Details
Brand Name
Taisn
Model Number
101
Place of Origin
China
Supply Type
OEM Service
Condition
New
Color
Silver
101 Metal-Filled Epoxy Putty Repair Adhesive, Casting Defect Rebuilding Putty Introduce

Taisn 101Casting Defect Rebuilding Putty

Double components, putty, general purpose. Used for repairing and restoring blowholes, shrinkage,

flow marks and cracks in castings with defect size more than 2mm. Can cure at low temperature and

humidity.

Package size

500g/set or 10kg/metal drum

Physical Properties

Color:Grey         
Specific gravity:1.65g/cm³
Mix ratio by weight:2:1
Mix ratio by volume:2:1
Working time(min):60min
Compressive strength(GB/T1041):98.0MPa
Tensile strength(GB/T6329):38.0MPa
Shear strength(GB/T7124):20.0MPa
Flexural strength(GB/T9341):65.0MPa
Hardness(GB/T2411):80Shore D
Cured time for machining:18h
Temperature range:-60~120ºC

Attention

1,When the temperature is below 15 ºC, some heating measures should be adopted; or the relevant curing time should be extended

2,When mix volume is more than 200g, the working time will be shorter

3,Above data is typical

Previous : Powder Coating Paint Stripper/Remover Next : Ground Calcium Carbonate CACO3 for Paint
Copyright 2023-2026 - www.globalbiz8.com All Rights Reserved