Hastelloy C22 PlateHastelloy C22 Plate UNS N06022 Plate Hastelloy C22 Machinability Hastelloy C22 AstmStandard specifications for ASTM B626 Hastelloy C22 Plate. If any specification is not mentioned here, you can contact us. We also manufacture and export any custom specification as per clients requirement.
Specifications | ASTM B626, ASME SB626 |
Dimensions | ASTM, ASME and API |
Size | Thickness 0.5-100mm |
Specialized in | Large Diameter Size |
Range | Width 1000-2500mm |
Type | plate |
Form | plate |
Length | Single Random, Double Random & Cut Length. |
End | Plain End, Beveled End, Threaded |
Hastelloy C22 ASTM B626 plate Chemical Composition
Grade | ASTM B626 Hastelloy C22 | |
---|---|---|
min | max | |
C | – | 0.010 |
Mn | – | 0.50 |
Si | – | 0.08 |
P | – | 0.02 |
S | – | 0.02 |
Mo | 12.5 | 14.5 |
Ni | Balance | Balance |
Cr | 20.0 | 22.5 |
Fe | 2.0 | 6.0 |
Co | – | 2.5 |
V | – | 0.35 |
W | 2.5 | 3.5 |
ASTM B626 Hastelloy C22 plate Mechanical Properties
Grade | ASTM B626 Hastelloy C22 | |
---|---|---|
Tensile Strength (MPa) min | Psi – 100000 , MPa – 690 | |
Yield Strength 0.2% Proof (MPa) min | Psi – 45000 , MPa – 310 | |
Elongation (% in 50mm) min | 45% |
Hastelloy C22 Welded Tube Physical Properties
Grade | ASTM B626 Hastelloy C22 | |
---|---|---|
Density | 8.69 g/cm3 | |
Melting Point | 1399 °C (2550 °F) |