Application:
l As-Cast Finish Concrete/bare concrete, early strength concrete ,high-endurance concrete
Appearance
White powder
Water Content (powder)(%)
≤4.0
Ph-value(20℃)(20% solution)
7.0~8.0
Concrete water reduction ratio(%)
≥14.0
Concrete Air Content(%)
≤3.0
Dosage Recommendation(%) in relation to weight of binder
Cement: 0.3~1.0%
Gypsum: 0.2%~0.5%