SVR 10 is made from field coagulum materials according to Standard Vietnamese Rubber. The materials are precleaned by passing them through creper - hammermills and then stored for some weeks for maturation before production. Mature materials are blended and soaked in the water to be cleaned, size reduced to crumbs, dried, and baled.
- Dirt: 0.1
- Ash content: 0.8
- Volatile matter: 0.8
- Nitrogen content: 0.6
- Initial Wallace Plasticity: 30
- PRI: 55
- Mooney: 70